Etch Rates for Micromachining Processing - Inst.eecs.berkeley.edu

7 downloads 46 Views 1MB Size Report
Kirt R. Williams, Student Member, IEEE, and Richard S. Muller, Life Fellow, IEEE. Abstract--- The ..... appear rough and insoluble white residues form for KOH.